You can see where around corners and even some straight runs it is peeling up. I’m running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I’ve trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

  • massacre@lemmy.world
    link
    fedilink
    English
    arrow-up
    3
    ·
    11 months ago

    buy a cheap spray / spritzer, fill it with IPA, saturate the hairspray before paper toweling it off. You may have to take two passes to get it right. You can get away with a pretty good layer of the the hairspray, so I usually just touch up the bed with a spray between builds and clean after maybe 10 or something…